| Magnetic Stripe |
● General
Characteristics: 
Coercivity Hc: 300 Oe, 650 Oe, 2750 Oe, or 4000 Oe,
etc.
Base film material: Polyester
Magnetic layer material:
Ferrite
Color: Black, Brown
Width: 12.5 mm
Length: 1090
meters
Base film thickness:(12±1)μm
Total thickness:(26~29)μm
●
Recommended Process Condition:
Laminate
Temperature:120~140℃
Pressure:10~15Mpa
Duration
time:20-25minute
The processing conditions are for the reference only.
The above parameters should be adjusted based on real working
conditions. |
|
|
|
|